On August 28th, China’s leading manufacturer of ultra-pure superalloys, large complex thin-walled high-temperature structural castings, deformed &casting superalloys JSNT Superalloy Material Technology Group released its first half-year financial report:
From January to June 2020, aviation revenue accounted for approximately 53.70% of main business revenue.
The company casts high-temperature alloys, including casting high-temperature alloys and precision castings, which are mainly used in the aviation field, large and complex thin-walled structural castings of aero engines, aerospace, ships, nuclear power, energy and other fields;
Wrought superalloys are processed into bars, tubes, wires, ribbons and other profiles according to customer`s requirements, which are mainly used in aviation, nuclear power, gas turbines and petrochemical fields;
Special stainless steel is mainly made of bars and tubes, and is mainly used in aviation and nuclear power fields.