TJTC Advanced Materials Technology Corporation is committed to R&D and production of high-performance precision alloy materials:
Materials:
FeCrCo permanent magnet alloy, soft magnetic alloy, elastic alloy, expansion alloy, resistance alloy, high temperature alloy, titanium alloy, special steel, stainless steel
Product form:
Precision wires, precision tubes, precision rods, precision tapes/ultra-thin foils and precision profiles.
Small diameter stainless steel seamless tube, capillary
The company has introduced advanced flat wire production lines, titanium alloy wire production lines, bright submerged arc welding wire production lines, and magnetic material production lines from abroad.
The varieties of precision strips include stainless steel, high temperature alloys, precision alloys, titanium alloys, etc.;
The wide and ultra-thin superalloy steel strip developed by the company for aerospace applications fills the technical gap of materials in related fields in China.